Hi Arun,
Try some perfluroinated solvents, for example Freon 113 and so on.
Good luck!

Xuemei

-----Ursprüngliche Nachricht-----
Von: Im Auftrag von Arun Kumar
Gesendet: Montag, 27. März 2006 07:42
An: [email protected]
Betreff: [mems-talk] Wet etchant for fluoropolymer

Hi all,

        I have a teflon like plasma deposited fluoropolymer(CF) film on
silicon substrate. I tried to etch the CF alone with acetone. It doesnt have
any etching on CF, is there any other chemical etchant that removes the CF
alone?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics