R Zhang, Electrical & Electronic Engineering
2006-04-12
[email protected]
2006-04-12
Brent Garber
anticorrosion material
Brent Garber
2006-04-12
I use anodized aluminum for all my RIE etching.  I get the aluminum
re-anodized once a year.  Watch out for that Bob Henderson guy!

Brent Garber

[email protected] wrote:

> aluminum or stainless steel won't etch and hold up real well to SF6
> Bob Henderson
>