I love to use ZnO as a sacrificial layer. It can be removed quickly
(within seconds) in any acid-water mixture (e.g. HCl:H2O 1:50 will remove
2um of ZnO within 30 seconds). You can deposit ZnO be sputtering using
either a ZnO target or a Zn target and N2O+Ar.
Of course Zn is not a very favorable material for many semiconductor
applications but it works great for MEMS.


Marco
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review