Metal contact to PMMA
2006-04-20
Basa Peter
2006-04-22
Kevin
Metal contact to PMMA
Kevin
2006-04-22
Hi Peter,

I am growing silver layers on PMMA and I have found e-beam evaporation
to work well.

Regards,

Kevin

On 4/20/06, Basa Peter  wrote:
> Hi,
>
> I'd like to make metal contact to a PMMA layer (on Si substrate).
> Anyone has an idea which is the best method to do that (evaporation,
> sputtering, etc.)? I don't want to harm the PMMA layer.