Dear members:

I plan to etch four square-shaped electrodes on the surface of a PVDF film.
I intend to purchase the PVDF film from either one or both manufacturers.
One of them provides its films with a Ni-Cu coating and the other coats them
with Ni-Cr alloy. Now my question comes at this point: which etchant is
appropriate in each case? Have you come across any commercially available
products suitable for this need? Do you have any particular recommendation?
Thank you.

Regards,

Ashkan Mirbagheri
Graduate student, Master of Applied Science
Mechanical & Industrial Engineering Department
Concordia University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics