MEMSnet Home: MEMS-Talk: how to reduce miscut angle
how to reduce miscut angle
2006-04-27
Andrea Mazzolari
2006-04-28
Duan
2006-04-28
Kenneth Smith
how to reduce miscut angle
Duan
2006-04-28
what do you exactly mean by saying miscut angle?

On 4/27/06, Andrea Mazzolari  wrote:
> I have (110) silicon waferds with a miscut angle of 0.1°. Is there a way to
> reduce miscut angle? Can an etching in TMAH help?
>