Hi friends,
        We have fabricated a Platinum RTD ( Pt 1000). Can anyone suggest
the standard methods being followed for testing this RTD.
        For your information, We have faricated Pt 1000 and out test range
is -90 deg. C to +55 deg. C.

        Please recomend any book, journal, literature etc. for this issue.

Thanks

     Kamal Kishore                     Phone :(0172) 2237401 to 10
     Engineer,VLSI:FAB                 Ext:576,550,570,441
     Semiconductor Complex Limited.    Fax:(0172)-2236378,2236885
     Sector 72(Indl.Area),S A S Nagar,
     Mohali, Punjab- 160071
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering