MEMSnet Home: MEMS-Talk: Nichorme thin film resistivity
Nichorme thin film resistivity
2006-07-21
T Zhu
Nichorme thin film resistivity
T Zhu
2006-07-21
Hi:

I'am doing some Nichorme thin film resistors, but the general information on the
internet of the resistivity of Nichrome was 1.1x10^-6, has anyone got any
information on resistivity of Nichrome thin film? say 50nm-100nm.

Thanks very much.

========
T Zhu
School of Engineering and Electronics
The University of Edinburgh,
King's Buildings,
Mayfield Rd,
Edinburgh
EH9 3JL
(Int +44) 131 650 5567 (enquiries),
(Int +44) 131 650 6554 (FAX)
MAIL1
========

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.