A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Indium evaporation
Indium evaporation
2006-08-04
[email protected]
2006-08-04
Shile
2006-08-04
B Frank
Indium evaporation
[email protected]
2006-08-04
Hello,
I am trying to e-beam evaporate .35 microns indium on silicon with Ti/Au
on it. I am getting milky looking film instead of a shiny, aluminum like
film.
I am using indium shots 99.9999% using a moly liner in a AJA system.
This oxide prohibits me to bond this In coated wafer to another Au coated
wafer.
Has anyone else encoutered the same issue with indium evap. How to get rid
of the oxide.
Any suggestion will be appreciated.

thanks
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing