Adhesives wafer bonding
2006-08-16
Cheng-Yu Hsieh
2006-08-16
Nicolas Duarte
2006-08-17
LSujatha
2006-08-19
David Henriks
2006-08-17
Lung-hao Hu
Adhesives wafer bonding
Cheng-Yu Hsieh
2006-08-16
Hi Everybody,
I am trying to bond one 4 inch silicon wafer to a 8 inch silicon wafer.
I need a temporary bonding adhesive which I should be able to remove
after I have done chemical mechanical planarization process on the 4 inch wafer.

Does anybody know of commercially available adhesives
that I can use for this? I need an adhesive which is
very  simple in it's application and ideally would
like something which I can just apply in-between the
two wafers and then stick them together and later
should be able to de-bond them easily too.

Cheng-Yu Hsieh

Institute of MicroElectroMechanical System , National Tsing Hua
University, 101, Sec. 2, Kuang-Fu Road,Hsinchu ,Taiwan 300 , ROC
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
University Wafer