MEMSnet Home: MEMS-Talk: 10 nanometer hole
10 nanometer hole
2006-08-17
[email protected]
2006-08-17
Roger Shile
2006-08-18
Isaac Chan
2006-08-19
Jacques Jonsmann
2006-08-20
Jeehwan Kim
2006-08-22
Glenn Silveira
2006-08-21
Glenn Silveira
Re: 10 nanometer hole
2006-08-18
mohendra roy
2006-08-21
Jim Beall
2006-08-19
[email protected]
2006-08-21
[email protected]
2006-08-21
Rob Knobel
2006-08-21
[email protected]
10 nanometer hole
Jeehwan Kim
2006-08-20
You can try diblock copolymer pattern and transfer this pattern to the film.

J.Kim
> -----Original Message-----
> Does anyone know how and who can make a 10 nanometer hole in a 50
> nanometer film.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing