Dear friends,
When I am doing KOH etching of Silicon with silicon dioxide mask in 30%
solution I am getting the black color in the place of silicon to be etched
and hence the etching starts very late. the etching time becomes almost
twice.Can anyone tell the reason for this black color formation? How to
avoid?
Temperature is 75 degrees Centigrade.
Suggestions please.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review
Addison Engineering