Dear all,

up to now I’m working with the photoresists Ormocer and SU8.

I have now the problem, that I need a resist of similar kind (optical
proparties, refractive index in the range of 1.4 to 1.6, illumination
wavelength in the range of 330 to 400nm) but with standard layer thikness
about 500nm (or even less). If possible the resist should have only few
losses at telecomunication wavelengths (1.55µm and 1.3µm) and
resolutions
down to 100nm should be possible. Further advantage would be few losses at
visible wavelengths but this is not stringent necessary.


Thanks in advance

Sven Passinger
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics