evaporation deposition
J.J wang
2006-09-25
1) Clean your glass wafer thouroughly.
2) Try a little bit thicker chrome
3) DON'T use ultrasonic

Good luck.

Rupesh Sawant  wrote: hi,
i tried to deposit Au on glass slide using eavpporation deposition method.
i deposited a 5 nm chromiun layer before depositing Au and then deposited
180nm Au layer. photoresist was used as a sacrifial layer. the Au layer
(along with the desired features) came out instantly when i dipped the slide
in acetone but the photoresist was still there on the slide.

could someone tell me a reson for this?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing