A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Etching Ag
Etching Ag
2006-09-28
Benyimin Hadad
2006-09-28
[email protected]
2006-09-28
PRAMOD GUPTA
2006-10-02
Peter Svasek
2006-10-27
Kevin
Etching Ag
Peter Svasek
2006-10-02
Hi,

we use a 40% solution of Fe(NO3)3 in water to etch Ag.

Regards
Peter

Benyimin Hadad wrote:

>Hello
>
>I want to know if someone know how to etch Ag , dry and wet .
>

Vienna University of Technology
Institute of Sensor and Actuator Systems
Gusshausstrasse 27-29/366
A-1040 Vienna
Austria

Tel. +43-1-58801-36643
Fax  +43-1-58801-36699



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing