MEMSnet Home: MEMS-Talk: Su8-2100 soft bake
Su8-2100 soft bake
2006-12-14
Barbara Cortese
2006-12-15
Gareth Jenkins
2006-12-15
GARCIA BLANCO Sonia
2006-12-18
st20000
Su8-2100 soft bake
Barbara Cortese
2006-12-14
Dear all

Recently we met a problem using SU-8 2100. When spinning (at 1000rpm),after
softbake treatment, waves appear on the layer. The hotplate I use is levelled,
and I am using as a substrate silicon. The soft bake lasts 15 minutes at 65°and
60 min at 95°. I tried longer times of soft bake but the problem is always the
same, and the layer is always soft.
Can you help me to solve this problem? What do you think the problem is caused
by?


Barbara Cortese


------------------------------------------------------
Passa a Infostrada. ADSL e Telefono senza limiti e senza canone Telecom
http://click.libero.it/infostrada14dic06


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation