MEMSnet Home: MEMS-Talk: RE: Shear strength of Gold on SU-8
Shear strength of Gold on SU-8
2006-12-22
Yue Mun Pun, Jeffrey
RE: Shear strength of Gold on SU-8
2006-12-28
Yue Mun Pun, Jeffrey
RE: Shear strength of Gold on SU-8
Yue Mun Pun, Jeffrey
2006-12-28
Hi all,

I am trying to fabricate a device which uses an in-plane two-arm cantilever to
rip apart a thin 100nm thick Gold bridge, which is evaporated onto the SU-8
cantilever.  This gold bridge stretches between the cantilever and another
platform also made of SU-8.

I have read that a thin film of gold (of thickness 300nm) has peak tensile
stress of 300MPa and experiences a strain of 0.05 before it breaks.  So the SU-8
cantilever needs to exert such a force on the Gold bridge to break it.

Since the gold also sits on the SU-8 and might be sheared off the SU-8 as the
cantilever moves laterally, I would like to ask whether anyone has any
information on the bond shear strength of Gold on SU-8 (I have read that the
bond pull strength of Gold on SU-8 is 4.8MPa, but I would like to know what the
bond shear strength is).


Mr. Jeffrey Mun Pun YUE


Division of Bioengineering
Block E3, #05-18, Nanobioanalytics Lab
9 Engineering Drive 1
National University of Singapore
Singapore 117576
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation
Harrick Plasma, Inc.