Dear Paolo,
PMMA can be used for photo/ionbeam/ electron beam lithography

On 1/10/07, paolo bondavalli  wrote:
>
> Dear members,
> I need some information abour PMMA.
> Is it used for photo-lithography?
> Is it photo-sensitive?
> Is it resistant to ethanol?
>
--
Ranjini Menon
Scientific Officer
VECC
Department of Atomic Energy
1/AF , Salt lake city
Kolkata
West bengal-700064
phone:033 2337 1230 extn 3204
fax: 033 2334 6871
e-mail: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer
The Branford Group