MEMSnet Home: MEMS-Talk: Copper plating
Copper plating
2007-02-03
Nik Dee
2007-02-04
Shay Kaplan
Copper plating
Shay Kaplan
2007-02-04
The copper diffuses into the gold

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Nik Dee
Sent: Saturday, February 03, 2007 4:19 PM
To: [email protected]
Subject: [mems-talk] Copper plating

Hi guys, I am currently using a Copper plating solution (Water, Copper
Sulphate, Sulphuric Acid, NaCl and CUbath copper brightener) on gold seed
layer. I try to keep the plating rate to 30mA / cm2. I have noticed
sometimes that the copper plated on the seed surface is not bright enough
and it gets a pink colour. Do you have any idea what the reason for that
might be?

Nik Dee
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing