MEMSnet Home: MEMS-Talk: Adhesion of evaporated Au on Pt layer
Adhesion of evaporated Au on Pt layer
2007-02-21
Rashed Mahameed
2007-02-21
Brent Garber
2007-02-22
Kirt Williams
2007-02-22
WANG,TAK
Adhesion of evaporated Au on Pt layer
Brent Garber
2007-02-21
Au will stick fine to Pt but I'm not sure how well if you are breaking
vacuum in between the 2 films.

Rashed Mahameed wrote:
> Hi everybody,
>
> Does anybody know if I can evaporate Au directly to Pt without
> adhesion layer (e.g. NiCr)? Is there a good adhesion between the two
> layers?
>
> I need to deposit a couple of microns of Au on Pt.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation