A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: AlGaAs microbeams cleaving??
AlGaAs microbeams cleaving??
2007-03-15
vaibhav mathur
2007-03-16
shay kaplan
AlGaAs microbeams cleaving??
vaibhav mathur
2007-03-15
I've fabricated an array of 50-400 microns long,two ends clamped AlGaAs
microbeams on GaAs substrate. Could someone suggest the best way to cleave
these beams precisely at desired lengths to form pairs of oppositely facing
cantilevers.Lasercutting is an expensive option, is there an alternate way
of doing this?

regards
Vaibhav Mathur
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing