MEMSnet Home: MEMS-Talk: PDMS is sticking better on microscop slides or on Si wafer?
PDMS is sticking better on microscop slides or on Si wafer?
2007-03-20
Petru Lunca Popa
PDMS is sticking better on microscop slides or on Si wafer?
Petru Lunca Popa
2007-03-20
Hi guys
I am depositing my circuit by litography either on glass or on SI
wafer The PDMS is sticking better on glass or on SI . It seems to
stick much easier on Si?

Petru