Pinholes in Evaporated Gold film
2007-03-23
Yue Mun Pun, Jeffrey
Ultra-thin silicon wafers
2007-03-24
Andrea Mazzolari
Ultra-thin silicon wafers
Andrea Mazzolari
2007-03-24
Hi all,
i'm looking for ultra thin silicon wafers (50um or less)

Do you have any suggestion where to buy them ?

Best regards,
Andrea