MEMSnet Home: MEMS-Talk: Under Bumb Metallization
Under Bumb Metallization
2007-04-14
Tolga YELBOGA
2007-04-15
Bill Moffat
Under Bumb Metallization
Bill Moffat
2007-04-15
Tolga,
           Simple production process by Hughes Carlsbad for years.  13 =
microns of resist, create lift off profile using image reversal then 7 =
microns of Indium for the bumps.  Totally repeatable for at least 7 =
years.  Contact me directly for more commercial details and technical =
papers.  [email protected]  Bill Moffat
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing