MEMSnet Home: MEMS-Talk: cutting the REMagnet , N48
cutting the REMagnet , N48
2007-04-22
LINA AYAT.
cutting the REMagnet , N48
LINA AYAT.
2007-04-22
Dear all
in my project i need to use a permanent magnet (REMagnet N48), I have no
idea how to cut this magnet to desire size considering not to damage the
magnetization features.the thickness is 790um and i need to cut it to half.

many thanks and regards;