bonded wafers dice
2007-05-09
kris
2007-05-09
Shay Kaplan
2007-05-09
David Nemeth
2007-05-10
P.E.M. Kuijpers
bonded wafers dice
Shay Kaplan
2007-05-09
If the bond is good - no problem. If it's going to fall apart - the bond is
bad.

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of kris
Sent: Wednesday, May 09, 2007 5:32 PM
To: [email protected]
Subject: [mems-talk] bonded wafers dice

Hello,

I was wondering if we can dice a Au-Au
thermocompression bonded wafer pair using the diamond saw.

I need individual dies from the wafer pair to go for the etch trails.

Your suggestions are highly appreciated.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer