MEMSnet Home: MEMS-Talk: Au-etchant attacking plated nickel
Au-etchant attacking plated nickel
2007-05-21
Sven Holmström
2007-05-21
David Nemeth
silicon nitride etch by koh?!
2007-05-21
Andrea Mazzolari
2007-05-22
Jordi Teva
2007-05-22
Shay Kaplan
2007-05-22
IGOR KADIJA
2007-05-22
Kirt Williams
Au-etchant attacking plated nickel
Sven Holmström
2007-05-21
Dear all,

We selectively plate nickel onto gold coated silicon wafers. Later we etch
the gold using standard gold etch (Aldrich, Potassium Iodide etchant). We
have sometimes problem with the gold etchant etching also the nickel.
According to data sheets and literature KI is not supposed to etch nickel
(for example Etch Rates for Micromachining Processing—Part II by Williams,
Gupta and Wasilik.).

The keyword is 'sometimes'. The behaviour is very erratic. We have produced
several nice pieces without any problems, but then at some times the nickel
is etched even faster than the gold! (the nickel etch also in general seem
uneven, etching from the sides in concentric half circles rather than
evenly). It seems to us like the nickel etching is mainly depending on the
individual nickel baths. We use all the time standard Nickel Sulphamate
baths, but since we mix them by hand slightly individual differences are
unavoidable. The concentric half circles also to tend to point  to
contaminations being a problem.

I wonder if anyone else has encountered this problem and in which direction
we should go to get control of the process.

regards,

/Sven Holmström, Koc University, Istanbul, Optical Microsystems Laboratory
(
http://mems.ku.edu.tr/)

Work phone: +90 212 338 1772
Mobile phone: 05383365642
FAX: +90-212-338-1548 (Please note my name)
E-mail: [email protected] 
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation