Hi everyone,

I have problem removing photoresist.
I spin coat AZ1518 on silicon, prebaked for 10min @ 90C, after develop, baked
for 20min @ 90C.
Then, I did some RIE with SF6/Ar/O2.  After that, I tried to ash it with O2
plasma for 20min but it didn't come off.  I also tried treat it in Photoresist
remover 1165 heated up to 70C for about 30mins, but nothing happened.  Does
harsher O2 plasma or does heating it up to hundreds of degree in oven help?

Any suggestions?

Thanks
Hao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing