Leyla Soleymani
2007-05-24
[email protected]
2007-05-24
Leyla Soleymani
Parylene patterning
Leyla Soleymani
2007-05-24
Hi Dirk,

thank you for your reply, by any chance do you know what should the ratio of
the resist thickness to parylene be?

Regards,
Leyla


On 5/24/07, [email protected]  wrote:
>
> Plasma etch and patience can do the job ;).
> Various oxygen plasma etch recipes for parylene have been reported (do
> eg a quick Google Scholar search on it).
> You can use resist as a mask but make sure it's (much) thicker than your
> parylene film; you can afterwards wash away the resist with acetone or
> your solvent of choice (the parylene will be inert in pretty much any
> solvent/etchant). I wouldn't recommend sonicating it though (depending
> on how good your parylene adheres to whatever your substrate is).
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.