A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Re BCB
Re: Re BCB
2007-05-24
saravan kallempudi
Re: Re BCB
saravan kallempudi
2007-05-24
I am working according to the DOW charts but increasing the temperature step by
step  slowly.
We
have the oven where we can increase the gas concentrations but havent
tried yet. I am using dry etch grade what about you? One more thing do
you have any dry etch recepies for BCB

Thanks in advance,
Sreenivasa Saravan

reply