RE: 2.5 um microchannels in SU-8 (shay kaplan)
2007-06-10
Dave
2007-06-11
Herman Walgraeve - TNW
2007-06-10
[email protected]
2007-06-11
Herman Walgraeve - TNW
RE: 2.5 um microchannels in SU-8 (shay kaplan)
Herman Walgraeve - TNW
2007-06-11
Hi Shay,

I am using straight developer.
Lithography is done with a chrome mask.

Herman.

________________________________

Van: [email protected] namens Dave
Verzonden: zo 10-6-2007 17:17
Aan: [email protected]
Onderwerp: [mems-talk] RE: 2.5 um microchannels in SU-8 (shay kaplan)

Are you using straight developer from the bottle or a dilution? 2.5 microns
is pretty damn small for near UV, i bet that the lithography process is your
problem. Are you direct writing or are you using a photomask?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review