Inquiry regarding sidewall deposition of wafers in e-beam metalization
2007-06-26
polly
Inquiry regarding sidewall deposition of wafers in e-beam metalization
2007-06-26
shay kaplan
Inquiry regarding sidewall deposition of wafersin e-beam metalization
2007-06-26
Bill Moffat
Inquiry regarding sidewall deposition of wafersin e-beam metalization
Bill Moffat
2007-06-26
I agree with Shay.  This is the reason that people use image reversal to
create a reverse slope on the resist side wall to preclude metal build
up on the resist side walls.

Bill Moffat, CEO
Yield Engineering Systems, Inc.
203-A Lawrence Drive, Livermore, CA  94551-5152
(925) 373-8353

[email protected]

www.yieldengineering.com


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of shay kaplan
Sent: Tuesday, June 26, 2007 12:51 PM
To: 'polly'; 'General MEMS discussion'
Subject: RE: [mems-talk] Inquiry regarding sidewall deposition of
wafersin e-beam metalization

In ebeam evaporation, the process is a line of site process. i.e. the
atoms / molecules fly on a straight line from the source to the surface.
For these reason, the thickness is proportional to the cosine of the
angle. A 90 deg wall will not get coated. However, in some systems the
wafers are tilted and are rotating during evaporation (planetary
fixture). In such a system one get can some material on the sidewall
depending on the system geometry

shay
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics