Hi Josh

How would be your evaporation rate?! so high?! Could it be an evidence
for noncontiguous deposition (some regions thicker than others over
your substrate). If your film is not so uniform, its resistivity will
be given by thinner regions. But it is only a fast kick, a don't know
if there are some kinds of interdifusion problems or else on your
system. If you really have a heterogeneous film, I think probably the
thermal features will be affected too.

Best wishes

NH
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing