MEMSnet Home: MEMS-Talk: Parameters for VHF-PECVD to plasma bond pdms to glass
Parameters for VHF-PECVD to plasma bond pdms to glass
2007-08-06
Vishwa
Parameters for VHF-PECVD to plasma bond pdms to glass
Vishwa
2007-08-06
Hi,
I am trying to use the VHF-PECVD to plasma(oxygen) treat pdms and
glass, to bond them. So far, I have had no luck. We have treid
(25mtorr, 25w, 2min), (25mtorr,25w.10sec) and (25mtorr,25w,10min).
None of these seem to help. Can any of you suggest what might be the
right parameters.

Thanks in advance
Vishwa
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation