MEMSnet Home: MEMS-Talk: solder deposition
solder deposition
2007-09-17
X.P. Zhu
solder deposition
X.P. Zhu
2007-09-17
Hi all,

   Which method below is best for depositing AuSn
solder on copper heatsink: e-beam or thermal
evaporation? And which is best for indium on copper?
Thank you.

X. P. Zhu