MEMSnet Home: MEMS-Talk: Nb wet etching
Nb wet etching
2007-09-22
Sadhana Patil
2007-09-24
Kirt Williams
2007-09-24
Edward Sebesta
2007-09-24
Roger Shile
Nb wet etching
Roger Shile
2007-09-24
Nb can be etched with SF6 plasma.  For wet etch HF can be used.

Roger Shile

-----Original Message-----


Hi all,
Looking for some help on the kind of wet etchants available for etching
Nb.
I have vaguely heard about HF(1):HNO3(1). Does anybody have an idea of
what is the etch rate of this chemical for Nb? Are there any other
etchants available for Nb? And does it etch other metals like Au, Fe,
CuMn, Ni?
Thanks,
ES...
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.