MEMSnet Home: MEMS-Talk: Poly Silicon Resistivity
Poly Silicon Resistivity
2007-09-27
Rana, Mukti M
2007-09-27
Suraj Patil
2007-09-28
Thomas Wolff (WEP)
Poly Silicon Resistivity
Suraj Patil
2007-09-27
Hi Mukti,

1. V.A. Gridchin, V.M.Lubimsky, M.P. Sarina, " Piezoresistive properties of
polysilicon films".
2. P. Kleiman et.al."thernmal drift of piezoresistive properties of PLCVD
polysilicon thin films between room temperature and 200 C.

I hope this helps.

Regards,
Suraj Patil


On 9/26/07, Rana, Mukti M  wrote:
>
> Hello,
>
> Can anyone suggest me the variation of resistivity of polysilicon with
> doping concentrations? Reference of any paper or article will be
> appreciated.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer