MEMSnet Home: MEMS-Talk: breakdown voltage in MEMS structures
breakdown voltage in MEMS structures
2007-10-12
ashwini jambhalikar
2007-10-12
shay kaplan
breakdown voltage in MEMS structures
ashwini jambhalikar
2007-10-12
Friends,
can somebody give me some reference about following problem:

if the gap between two electrodes,is 5 micron / 8 micron/10 micron
what voltage can be safely applied for electrostatic actuation,
considering air or argon or nitrogen as dielectric.
Ashwini