MEMSnet Home: MEMS-Talk: dilute SU8-100 with GBL
dilute SU8-100 with GBL
2007-10-21
nuaaljf
dilute SU8-100 with GBL
nuaaljf
2007-10-21
   hello everyone:I would like to get a 5um coating with SU8, so I have to
dilute SU8-100 with GBL. I want to know the GBL got from common chemical
store(not Micro Chem Corp.) can be used? and I want to know the steps to dilute
SU-8 with GBL.Best regardLi Jinfeng