MEMSnet Home: MEMS-Talk: Striations during spin-coating
Striations during spin-coating
2007-10-24
Sandip Agarwal
2007-10-24
Matthew Walker
2007-10-24
Sandip Agarwal
2007-10-24
dbp lists
2007-10-25
Kevin Paul Nichols
2007-10-26
Nicolas Duarte
2007-10-25
Pablo de la Fuente
2007-10-25
Nodes Norbert
Striations during spin-coating
Sandip Agarwal
2007-10-24
I am trying to spin-coat a polymer (1% PMMA-butadiene copolymer in
toluene) on a substrate that has topographical features that are 50x50
micron posts and 10 microns tall. I observe striations or ripples that
run from the center of the substrate to the periphery after
spin-coating. Any solutions? I have tried varying the concentration and
dynamic dispensing without any success.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing