MEMSnet Home: MEMS-Talk: Deep Quartz etch
Deep Quartz etch
2007-11-29
Haixin Zhu
Deep Quartz etch
Haixin Zhu
2007-11-29
Hello,

We have been trying deep quartz etch (20-40um) using HF mixture for a
while, and could not find a suitable etch mask for this purpose. Though
lot of people suggest the use of Au/Cr layer, we have the problem
getting very dense and high-quality Au film. Is there any comments or
suggestions on the selection of etch mask?

Thanks

Haixin