Chromium reaction in DRIE (Bosch)?
2008-02-06
Sven Holmström
2008-02-06
Nodes Norbert
2008-02-06
Sven Holmström
Chromium reaction in DRIE (Bosch)?
Sven Holmström
2008-02-06
On Feb 6, 2008 5:24 PM, Nodes Norbert  wrote:
> Hello Mr. Holmström.
>
> Even after removal with a suitable solvent, a very thin Cytop polymer layer
can remain on top of chrome and inhibit etching.
> You may have to treat the surface with some plasma or ashing process before
chrome etching.

Thank you for your answer. This might very well be the reason. The
only reason not to believe this is that the surface gold could be
etched. But the Cytop might of course stick better to Cr than to Au.

I will try plasma treatment.

/Sven
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.