A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Electromagnetics
Electromagnetics
2008-02-15
Hakemi, Ghazal
2008-02-18
Morten Aarøe
2008-02-18
Hong Chen
2008-02-19
David Nemeth
2008-02-20
Morten Aarøe
2008-02-21
Satyanarayan Nagarajan
2008-02-21
Morten Aarøe
Electromagnetics
David Nemeth
2008-02-19
No, that's the dielectric constant.  The magnetic permeability should be 1
or very close to it.

David Nemeth

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Hong Chen
Sent: Monday, February 18, 2008 11:12 AM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] Electromagnetics

Hi Ghazal,

It is 11.7~11.8 for Si.

Hong
URI

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Hakemi, Ghazal
Sent: Friday, February 15, 2008 10:18 AM
To: [email protected]; [email protected]
Subject: [mems-talk] Electromagnetics

Dear all,

Does anybody know what the relative permeability of Silicon is? I need to
implement it in one of my simulations.
It seems impossible to find!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics