MEMSnet Home: MEMS-Talk: Titanium etch
Titanium etch
2008-03-07
Michael Cooke
2008-03-07
Brent Garber
2008-03-08
Deepasree Konduparthi
Titanium etch
Michael Cooke
2008-03-07
Dear all,

I was wondering if there is a safer etch for Titanium which I haven't
come across which doesn't involve HF or HF as a biproduct. Ideally it
should be done at room temp.

Cheers

Dr Michael Cooke
Electronic Device Process Technologist
reply