Re: KOH etching for (110) silicon wafer
1998-08-26
Arum Han
1998-08-19
Michel Rosa
1998-08-20
Dong-il Dan Cho
1998-08-26
Arum Han
Re: KOH etching for (110) silicon wafer
Arum Han
1998-08-26
Refer Journal of The Electrochemical Society Vol. 147
Number 7, July 1998 "Aqueous KOH Etching of Silicon (110)"
by 'Byoungwook Kim and Dong-il Dan Cho', pp. 2499.

--------------------------------------------
Arum Han
Center for Microelectronic Sensors and MEMS
University of Cincinnati
E-mail  : [email protected]
Address : 688 Riddle Rd. #400c
          Cincinnati Ohio 45220
          USA
Phone   : (513)-556-4795 (Office)
          (513)-872-0710 (Home)
------------------------------ ------------


On Wed, 19 Aug 1998 [email protected] wrote:

>  Dear MEMS
>  I have worked (110) silicon wafer KOH etching  verticaly for
> acceleration sensor.
>   But vertical KOH etching was not conformed. I want to know the
> method for  vertical KOH etching.
>   I wish your advices and good informastions.
>  Thanks for reading my e-mail.
> email adress; [email protected]
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group