MEMSnet Home: MEMS-Talk: PDMS micro channel problem
PDMS micro channel problem
2008-03-27
vidhu g
2008-03-27
Kevin Paul Nichols
PDMS micro channel problem
Kevin Paul Nichols
2008-03-27
Dear Vidhu,

Could you explain your problems in more detail?

- Kevin

On 3/27/08 4:24 AM, "vidhu g"  wrote:

> hi all
>
> I'm pursing project in BIOMEMS. I have got a problem in loading a
> sample into PDMS micro channel and tagging a Polyclonal PSA Ab to
> 20nm gold nanoparticles. Can any one explain methods to solve my
> problems.

Kevin Paul Nichols
MESA+ Institute for Nanotechnology
Mesoscale Chemical Systems
Meander 151
University of Twente
Postbus 217
7500 AE Enschede
The Netherlands

Office: +31 (0)53 489 26 31
Mobile: +31 (0)6 49 312 471
Fax   : +31 (0)53 489 35 95
Email : [email protected]
Web   : http://mcs.tnw.utwente.nl/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering