MEMSnet Home: MEMS-Talk: Hydrophobic treatments/coatings for Polycarbonate
Hydrophobic treatments/coatings for Polycarbonate
2008-04-09
Paul Monaghan
2008-04-09
Adrian Brozell
2008-04-09
Paul Monaghan
2008-04-09
Boris Kobrin
2008-04-10
Paul Monaghan
Hydrophobic treatments/coatings for Polycarbonate
Adrian Brozell
2008-04-09
Oxidation makes it hydrophilic.  Polycarbonate should be reasonably
hydrophobic like most plastics.

adrian

Paul Monaghan wrote:
> Hi,
>
> Is there anyone that could point me in the direction of some simple lab
> methods for changing the surface wettability of polycarbonate -
> coatings/treatments etc.
>
> I would like to make it more hydrophobic than its native state whilst
> retaining the polymer's bulk properties. I can plasma oxidize the surface
> if that helps?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.