A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: my PDMS is not sticking anymore on SIO2
my PDMS is not sticking anymore on SIO2
2008-05-27
Petru Lunca Popa
2008-05-28
Kirt Williams
my PDMS is not sticking anymore on SIO2
Petru Lunca Popa
2008-05-27
Starting from 3 weeks ago I have problems with sticking PDMS on Silicon Oxide.
I checked all again. I didnt change any parameters but sudenlly
stopped to stick . I check the expiration date and all parameters
Any ideea what can be ?
I am using Sylgard 184 from Dow Corning  10 to 1 ratio between part A and B

Thanks a lot
Petru
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing