Question about EDP etching
1998-08-21
mabin
1998-09-11
mabin
Question about EDP etching
mabin
1998-09-11
Dear colleagues:
I am using EDP(ethylenediamine-pyrocathecol-water) to etch <100> silicon
but the uniformity is not good and I don't know how to control the etch
rate. Does any one like to tell me a typical composition for  EDP,
operating temperature and the relation between the etch rate and mol
concentration of each reagent. By the way, any one has the experience of
etching P++ silicon bridge out of the <100> N type silicon substrate
using EDP? Thanks in advance for any help.
--
Ma Bin
500, Yu Tian Road
Shanghai Institute of Technical Physics
The Chinese Academy of Sciences
Shanghai 200083
P.R.C.

Email: [email protected]
Tel: 86-021-65420850-13323(13127)


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
MEMS Technology Review