keeping PDMS level
2008-06-25
Jose Guevarra
2008-06-26
Sarosh Khwaja
2008-06-26
Bill Moffat
2008-06-26
[email protected]
2008-06-26
Mohd.Yusuf
keeping PDMS level
[email protected]
2008-06-26
Hey,

You can put the pdms in an oven at 80oC and it will solidify in ~30 minutes.
I know of people who do the same at 150oC.

Octavio Mondragon

> How about vacuum baking to extract solvent rapidly.  Bill Moffat
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]] On Behalf Of Sarosh Khwaja
> Sent: Thursday, June 26, 2008 2:10 PM
> To: [email protected]; General MEMS discussion
> Subject: Re: [mems-talk] keeping PDMS level
>
> Just an idea, how about spinning it at a very low RPM?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing